Gas welding The thermal power of the oxygen-acetylene gas welding flame is low and the heat is dispersed, so the weldment deforms greatly and the productivity is low. Preheating is required when welding thicker aluminum weldments with gas welding. The weld metal after welding not only has coarse grains and loose structure, but is also prone to defects such as aluminum oxide inclusions, pores and cracks. This method is only used for welding repair of unimportant aluminum structural parts and castings with thickness ranging from 0.5 to 10mm.

 